Non-Corrosion Resisting Steel DTD 5082


Technical Data Sheet

 

Chemical Composition Limits
Weight% C Si Mn P+S max Cr Mo Ni
DTD 5082 0.18-0.26 0.10-0.35 0.40-0.80 P 0.020
S 0.015
0.80-1.20 0.15-0.25 0.50 max
Other Chemically similar Specifications
Weight% C Si Mn P+S max Cr Mo Ni
AFNOR 25C04 0.22-0.28 0.10-0.40 0.60-0.90 P 0.035
S 0.035
0.85-1.15 0.15-0.30 -
WS 1.7218 0.22-0.29 0.15-0.40 0.50-0.80 P 0.035
S 0.035
0.90-1.20 0.15-0.30 -

Typical Mechanical Properties

Grade Yield Strength (0.2% Offset) Tensile Strength Elongation % min
hbar tonf/in² hbar tonf/in²
DTD 5082A 88 min 51 min 115 min
130 max
75 min
85 max
8

Availability
Alloy DTD 5082 A. For all stock availability contact Sales.

Customer Reviews - What Customers Say About Us!

"Just wanted to say thanks for your efforts and updates"
"I always try you as you often keep stock that can't be found elsewhere"
"Prompt answer & knowledge of available material, timescale & price within a good time"
"Packaging is superb"
"Thank you for your quick response"
  CLICK HERE TO VIEW OUR BROCHURE  

Disclaimer
Every effort is made to ensure that technical specifications are accurate. However, technical specifications included herein should be used as a guideline only. All specifications are subject to change without notice.