Aluminium Alloy 1350

Technical Data Sheet


Chemical Composition Limits
Weight% Si Fe Cu Mn Mg Cr Zn B Ga V+T Cr+Mn+Ti+V Others
1350 0.1 0.40 0.05 0.01 - 0.01 0.05 0.05 0.03 0.02 - 0.03 (each)
0.10 (total)
0.25 0.40 0.02 - 0.05 - 0.05 - - - 0.03 0.03 (each)

Aluminium Alloy 1350 has the minimum aluminium content of 99.5 %. Alloy 1350 is a non-heat treatable and is the alloy of choice for electrial condutors. This alloy has excellent formability and corrosion resistance. Alloy 1350 is used in various applications but its main uses are electrical conductors pins, rods, and rivets. This alloy can also be found in various wire form and clips where strength is not as important as economics. NB: 1350 has a tigher chemistry specification and is therefore often used in stead of 1050A.

Typical Mechanical Properties


Material Temper Tensile Strength (N/mm²) Elongation in 50mm
1350 Bar M 60 min 23
1350 Bar H2 85 (min) 13

Aluminium Alloy 1350 available in Bar, Drawn Strip, Wire and Solid Conductor. For all stock availability for Aluminium 1350 contact Sales.

Similar Specifications:
Al 99.5
Duricilium-T (Elect.)
BS 2897
BS 2898


More News ........ Cutting Capabilities Expanded
We have a brand new 3 metre Guillotine. Take a look:
Aircraft Materials Metal Cutting Durma VS 3006



Every effort is made to ensure that technical specifications are accurate. However, technical specifications included herein should be used as a guideline only. All specifications are subject to change without notice.